What is plastisol ink?

Published , by the PrintBlob team.

Plastisol is a screen-printing ink made of pigment suspended in a liquid plastic, and it stays liquid until it is heated, when it fuses into a solid film on the fabric. It is the most widely used ink for printing shirts, because it can be left in the screen for days without drying and is ready to print straight from the tub.

Its two defining traits for a shop are opposite sides of one fact: it is a thick, opaque layer of plastic sitting on top of the fabric. That gives bright colour on dark shirts and also a print you can feel.

How it behaves

ScreenPrinting.com describes plastisol as a “100% solid ink system” with essentially no solvent, and notes that more than 90 per cent of the time it is used as supplied. Compared with water-based ink:

Plastisol Water-based ink
Drying in the screen Does not; can sit for extended periods Can clog open mesh quickly, so screens are cleaned between sessions
Feel A film you can feel; higher opacity gives more Softer
Opacity Transparent to very opaque grades Generally less opaque
Cure Heat only briefly at about 300 to 330 °F Heat held until all water has evaporated
Emulsion Any Needs a water-resistant one

Leftover plastisol can go back in the tub; Screen Printing Magazine lists the cons as smearing under an iron or other heat source, and the need for solvent clean-up and correct disposal of waste.

Cure, and how to be sure of it

The usual target is about 320 °F (160 °C) for standard inks; low-cure plastisols are made to cure as low as 260 °F, which helps on heat-sensitive fabrics. What matters is the temperature of the whole ink layer, not of the air in the dryer, and thick deposits take longer. A laser thermometer reads only the surface; a donut probe measures inside the ink film, which ScreenPrinting.com prefers. If a print is under-cured it washes out, so wash-test a sample from every new combination of ink, garment and dryer: see curing and wash fastness.

Choosing the grade

  • Opaque grades for dark shirts, often over a white underbase. Opacity comes mainly from pigment load, so thin process-colour inks do not show on dark fabric: see ink opacity.
  • Low-bleed grades for polyester and blends, which block dye from the fibres: see dye migration.
  • Soft-hand additives to reduce the weight of the film: see hand feel.