What is screen printing emulsion?
Published , by the PrintBlob team.
Emulsion is the light-sensitive liquid coated onto a screen’s mesh and dried; exposed to light through a film of the artwork, it hardens everywhere except under the design, and the soft, unexposed part is washed out to leave open mesh that ink can pass through. The hardened emulsion is the stencil.
Choosing it is a decision about exposure speed, forgiveness and which ink you will use, and it is the part of screen making that fails invisibly until the stencil breaks down on press.
The three kinds
The table follows Thrive Screen Printing’s guide, with the exposure and wavelength notes from Screen Printing Magazine.
| Diazo | Photopolymer | Dual-cure | |
|---|---|---|---|
| Suits | Beginners, tight budgets, varying exposure conditions | High-detail work that needs precise reproduction | Most applications; precision with forgiveness |
| Exposure | Slow, wide latitude | Fast, narrow latitude, needs calibrated equipment | Medium speed, wide latitude |
| Shelf life | About 6 to 8 weeks after the sensitizer is mixed | Long | Not stated |
| Solids | Lower | Highest, with low viscosity | High |
| Mixing | Needed | Ready to use | Needed |
| Cost | Lowest | Highest | Medium |
Plastisol is compatible with all three. Water-based ink is not: it requires a water-resistant emulsion such as Chromaline Hydro-X, Ecotex PWR or SAATI Textil PHW Red, because ordinary emulsion can melt within minutes of contact. See water-based ink.
Coating and drying
- The emulsion layer over the mesh should be 10 to 20 per cent of the mesh thickness.
- The screen room should be 30 to 40 per cent relative humidity and 60 to 80 °F (15 to 27 °C); humidity above 50 per cent weakens the bond.
- Forced-air drying removes moisture more consistently, and the screen should be thoroughly dry before exposure, since water interferes with diazo crosslinking.
Matching emulsion and light
LED exposure units peak at 385 or 395 nm, and common emulsions and capillary films are sensitive at those wavelengths; diazo systems bleach from yellow during exposure, which gives a visual cue. SBQ systems are judged by stencil softness on the squeegee side and by loss of resolution, which signals overexposure. The unit and the times are covered in exposure unit.
Thick stencils and removal
For raised, high-density prints the stencil is built from capillary film of 200 to 400 microns, applied with direct emulsion, not water, because water thins the stencil and can make the film lift. See high-density ink. At the end of a job the emulsion is stripped so the frame can be recoated: screen reclaiming. Remover must never dry on the screen, because it can lock the emulsion into the mesh.
Sources
- Thrive Screen Printing: Which emulsion is right for me?, read 28 Oct 2026
- Screen Printing Magazine: Getting the best results from your LED exposure system, read 28 Oct 2026
- Screen Printing Magazine: Mastering high-density inks, read 28 Oct 2026
- ScreenPrinting.com: Emulsion remover and reclaiming, read 28 Oct 2026