What is high-density (HD) ink?

Published , by the PrintBlob team.

High-density, or HD, printing builds a raised design with sharp, vertical edges by pushing a thick ink through a stencil that is itself thick, so a lot of ink lands on the shirt in the exact shape of the artwork. Unlike puff, which expands under heat, HD gets its height from the stencil.

For a shop it is a premium finish: a logo you can feel, with an edge you can see, that adds real set-up work.

Building the stencil

Screen Printing Magazine’s feature on HD inks describes the method:

Step Detail
Film Capillary film from 100 to 1,000 microns; the most popular range is 200 to 400 microns
Attaching Direct emulsion, not water, because water thins the stencil and can make the film delaminate
Emulsion An SBQ-sensitised pure photopolymer; one coat with a squeegee to attach the film, then a double coat from the inside with a round-edge scoop coater
Drying About 1 hour in a heated cabinet; several hours or overnight without one
Exposure Metal-halide lamp of 3,000 to 6,000 W, 90 seconds per 100 microns of film, so 6 minutes for 400 microns; avoid fluorescent units, and test LED units first
Washout Optional 5-minute water soak, then wash the film side only with a pressure washer of about 1,000 psi, from about 1 foot, and vacuum dry
Mesh About 80 to 83 threads per inch, 70 to 71 micron thread, roughly 60 per cent open area

Weak lights give long exposures and poor edges, which is why the article prefers a strong metal-halide source: see exposure unit and emulsion.

Inks

HD inks are usually plastisol, used straight from the can, commonly in black and white and mixable for other colours; the cured finish is matte with sharp edges. HD gels are clear or contain particles and cure glossy with rounded edges, and if undercured they look like matte HD ink. HD bases need toner for colour, and some rise like puff. Water-based raised inks also exist.

Printing and curing

  • Off-contact is set higher than normal, and raised slightly for each successive HD screen.
  • Order. On mixed jobs, print the HD colours last.
  • Squeegee. A soft 55/90/55 triple-durometer blade, a deep angle, minimal pressure and one stroke; a second stroke can smear.
  • Flash quickly, then cure at 325 to 380 °F through the whole ink layer, slowing the conveyor so heat reaches the thick deposit. Glossy HD ink after curing usually means too much heat.

What does not suit it

The article warns that overheating can scorch white shirts, that performance fabrics and other heat-sensitive materials are poor fits, and that heavy deposits make clean prints difficult. A thick print also has a pronounced hand feel; say so on the product page.

Sources